Re: PO has me PO'd
Quote:
Originally Posted by Grounded63
No, it's made for hanging ( mostly non structural ) body panels. Gluing some pinch seams together in place of spot welding.
But, it shouldn't be used like a filler or have an exposed Seam in the middle of a exterior painted panel. Like if it was used to fill the roof to B pillar lead seam on a car. Or like a partial lower quarter panel replacement that was flanged. If the panels were panel bonded at the flange and the seam was filled in with panel bond. Then just sanded flat, epoxied, 2k surfacer, blocked, sealed, top coated, cleared. That " exposed " panel bond Seam has a tendency to " shadow " through the primer/top coats.
|
Thanks for the explanation
__________________
Semper Fi...Uncle Sam, you da man
All parts offered to help are free, unless otherwise noted
Dont try this stuff in my build thread, unless you have 55 years of mechanical OTJ training
SAFETY FIRST