08-13-2004, 06:24 AM | #1 |
Registered User
Join Date: Mar 2004
Location: Aviano, Italy
Posts: 221
|
Polishing The Grill
OK, 72 Cheyenne outer grill, best way to polish? Mine has no dents or dings but looks like went to town with sandpaper and it is all scrathed. How can you make them look better?
Is it Alum. or steel? |
08-13-2004, 06:25 AM | #2 |
Registered User
Join Date: Mar 2004
Location: Aviano, Italy
Posts: 221
|
boy, i need to proof read 1st...
|
08-13-2004, 07:12 AM | #3 |
67-72 Addict!
Join Date: Feb 2002
Location: The TAX State!
Posts: 7,857
|
Here's a link to a site that explains a method that should work. He did my fathers grille and it turned out awesome!
http://www.ieasysite.com/starquestri...strims_006.htm
__________________
Jim 1970 C/10 Fleetside w/Ghost Flames Lowered 4.5" front and 4" rear (Raked) 355/350 Turbo w/shift kit 10" Redneck Performance Verter w/2500 stall Hooker Super Comps part#2808-1 Performer RPM Air-Gap 12 Bolt w/3:73 gears- Eaton Posi Comp Cams XE262 with 1.6 Crane Energizers, Road Demon 625 and Brodix IK 180 heads |
08-13-2004, 07:20 AM | #4 |
Registered User
Join Date: Aug 2003
Location: Bonner Springs, KS
Posts: 311
|
The '72 outer grill surround is made of anodized aluminum. Anodizing is a process whereby aluminum is subjected to a chemical bath/electric charge. This creates a thin layer of oxidation that protects it from further corrosion. You can try to remove this coating by sanding or you can remove it with a caustic cleaner. I have heard that ez-off oven cleaner will do the job pretty easily. However, once removed, the aluminum is no longer protected from corrosion. It will polish up nicely, but will have to be frequently polished to keep it shiny. Or, you can have it re-anodized. I have read a few articles on the internet about "Home anodizing" and it doesn't look like it would be very difficult. Re-anodizing does require some nasty chemicals though.
TP |
08-13-2004, 09:40 AM | #5 |
Registered User
Join Date: Jan 2000
Location: Wyoming USA
Posts: 2,446
|
I am currently going through this process on my 69,I used easy-off oven cleaner with a scotch brite pad.Next I started sanding with 600 grit wet ,then I went to 1000 grit wet sand and next i'm gonna do the 1500 grit my grilll looked like it sat in a sand storm before and now it looks alot better than it did but not perfect.I am gonna use an buffing wheel on it next to bring the shine back
__________________
2001 Silverado K-1500 2005 FXDWG stage3 69 CHEVY Short/Step 327/4L60 373 posi 63 IMPALA 327 |
08-13-2004, 12:11 PM | #6 |
Registered User
Join Date: Jan 2003
Location: Seattle WA
Posts: 1,466
|
This was a good post...http://67-72chevytrucks.com/vboard/s...8&page=1&pp=25
__________________
FocuzTech Performance Evergreen Protective Coatings Gatorhyde...the best kept secret in spray in bed lining & protection |
08-13-2004, 05:03 PM | #7 |
Resident Young Old Dude !
Join Date: Jul 2001
Location: Nevada
Posts: 1,948
|
I did a "How to" a couple of years ago, with pictures. But it was lost in a changeover of servers. My grille has been Unprotected for going on three years. All I would have to do is hit it with some Polish. I had quite a few dents in mine, no holes, I worked it just like body work, and sanded the high spots of the dents with sand paper to smooth it out. Then as with anything else, sand with smoother grit until you can use polish to finish it up. Different people have different ideas on a daily driver, I did just the outer grille, As I had installed a billet inner.
Last edited by RON WOODGEARD; 08-13-2004 at 05:07 PM. |
08-14-2004, 02:34 PM | #8 |
Registered User
Join Date: Mar 2004
Location: Aviano, Italy
Posts: 221
|
Thanks guys, since the wife now claims the truck, guess she will do the sanding...
|
Bookmarks |
|
|